Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.47 g/cm³ Show Supplier Material materials with Dichte of 1.47 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 228 MPa Show Supplier Material materials with Biegefestigkeit of 228 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 9.65 GPa Show Supplier Material materials with Biegemodul of 9.65 GPa | ASTM D790 |
Dehnung | 23.0 °C | 2.5 % Show Supplier Material materials with Dehnung of 2.5 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 130 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 130 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 183 MPa Show Supplier Material materials with Zugfestigkeit of 183 MPa | ASTM D638 |
Thermisch
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 1.00E+15 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.00E+15 Ω·m |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.3 % Show Supplier Material materials with Schrumpfung of 0.3 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Application areas | Scooter, bearing, fender, bumper, water tank, car handle, bicycle, fuel tank, frame, refrigerator housing, etc | |
Fillers | 40% Glass Fiber |