Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.22 g/cm³ Show Supplier Material materials with Dichte of 1.22 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 93 MPa Show Supplier Material materials with Biegefestigkeit of 93 MPa | |
Biegemodul | 23.0 °C | 6.89 GPa Show Supplier Material materials with Biegemodul of 6.89 GPa | ASTM D790 |
Dehnung | 23.0 °C | 2 % Show Supplier Material materials with Dehnung of 2 % | ASTM D638 |
Härte, Shore D | 23.0 °C | 112 [-] Show Supplier Material materials with Härte, Shore D of 112 [-] | ASTM D785 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 96 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 96 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 68.5 MPa Show Supplier Material materials with Zugfestigkeit of 68.5 MPa |
Thermisch
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | ASTM D147 |
spezifischer Widerstand | 23.0 °C | 3.00E+16 Ω·m Show Supplier Material materials with spezifischer Widerstand of 3.00E+16 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | car bumper,Tube, switch box, fan motor cover, refrigerator back cover, motor support cover, TV shell, refrigerator lining, drawer, soymilk machine cover, electric kettle shell etc | |
Fillers | 40% Glass Fiber |