Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.52 g/cm³ Show Supplier Material materials with Dichte of 1.52 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 198 MPa Show Supplier Material materials with Biegefestigkeit of 198 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 8.06 GPa Show Supplier Material materials with Biegemodul of 8.06 GPa | ASTM D790 |
Dehnung | 23.0 °C | 2.6 % Show Supplier Material materials with Dehnung of 2.6 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 126 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 126 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 138 MPa Show Supplier Material materials with Zugfestigkeit of 138 MPa | ASTM D638 |
Thermisch
Technological properties
Property | ||
---|---|---|
Application areas | LED lamp Housing,Switch, socket etc | |
Fillers | 30% Glass Fiber |