Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.56 g/cm³ Show Supplier Material materials with Dichte of 1.56 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 180 MPa Show Supplier Material materials with Biegefestigkeit of 180 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 12 GPa Show Supplier Material materials with Biegemodul of 12 GPa | ASTM D790 |
Dehnung | 23.0 °C | 1.6 % Show Supplier Material materials with Dehnung of 1.6 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 78 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 78 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 130 MPa Show Supplier Material materials with Zugfestigkeit of 130 MPa | ASTM D638 |
Thermisch
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | ASTM D147 |
Surface resistivity | 23.0 °C | 1.00E+16 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+16 Ω/sq |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.3 % Show Supplier Material materials with Schrumpfung of 0.3 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Application areas | Automobiles, electronic appliances and home appliances,Connector, switch, DVD laser head, coil frame, gearbox, circuit board, lamp holder, reflector lamp cup and bracket, throttle body, junction box, oil pump impeller, valve body, LED lamp housing, thermal circuit board, heat dissipation element etc | |
Fillers | 30% Glass Fiber |