Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.39 g/cm³ Show Supplier Material materials with Dichte of 1.39 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegefestigkeit | 23.0 °C | 179 MPa Show Supplier Material materials with Biegefestigkeit of 179 MPa | ASTM D790 | ||
Biegemodul | 23.0 °C | 6.21 GPa Show Supplier Material materials with Biegemodul of 6.21 GPa | ASTM D790 | ||
Dehnung | 23.0 °C | 15 % Show Supplier Material materials with Dehnung of 15 % | ASTM D638 | ||
Härte, Shore D | 23.0 °C | 72 [-] Show Supplier Material materials with Härte, Shore D of 72 [-] | ASTM D785 | ||
Impact strength, Charpy notched, ASTM | 23.0 °C | 150 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 150 J/m | ASTM D256 | ||
Zugfestigkeit | 23.0 °C | 65 MPa Show Supplier Material materials with Zugfestigkeit of 65 MPa | ASTM D638 | ||
Reißfestigkeit | 12.0 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 178 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 178 °C | ASTM D648 | |
Entflammbarkeit | UL94 HB |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 16 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 16 kV/mm | ASTM D147 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic plugs, auto parts, mechanical parts, ships, aerospace, electronic housing etc | |
Fillers | 30% Glass Fiber |