Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.22 g/cm³ Show Supplier Material materials with Dichte of 1.22 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Dehnung | 23.0 °C | 85 % Show Supplier Material materials with Dehnung of 85 % | ASTM D638 | ||
Härte, Shore D | 23.0 °C | 110 [-] Show Supplier Material materials with Härte, Shore D of 110 [-] | ASTM D785 | ||
Zugfestigkeit | 23.0 °C | 47 MPa Show Supplier Material materials with Zugfestigkeit of 47 MPa | ASTM D638 | ||
Biegemodul | ASTM D790 | ||||
Reißfestigkeit | 47.0 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 178 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 178 °C | ASTM D648 | |
Entflammbarkeit | UL94 HB |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.3 % Show Supplier Material materials with Schrumpfung of 0.3 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic plugs, auto parts, mechanical parts, ships, aerospace, electronic housing etc | |
Fillers | 20% Glass Fiber |