Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.99 g/cm³ Show Supplier Material materials with Dichte of 0.99 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegefestigkeit | 23.0 °C | 35 MPa Show Supplier Material materials with Biegefestigkeit of 35 MPa | ASTM D790 | ||
Impact strength, Charpy notched, ASTM | 23.0 °C | 68 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 68 J/m | ASTM D256 | ||
Zugfestigkeit | 23.0 °C | 31 MPa Show Supplier Material materials with Zugfestigkeit of 31 MPa | ASTM D638 | ||
Biegemodul | ASTM D790 | ||||
Reißfestigkeit | 24.0 |
Thermisch
Rheological Properties
Property | Temperature | Value |
---|---|---|
Schrumpfung | 23.0 °C | 1 - 1.5 % Show Supplier Material materials with Schrumpfung of 1 - 1.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Flame-retardant V0, halogen-free ring, TV parts, electrical parts, holiday lights, Christmas lighting |