Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.16 g/cm³ Show Supplier Material materials with Dichte of 1.16 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 110 MPa Show Supplier Material materials with Biegefestigkeit of 110 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 3.9 GPa Show Supplier Material materials with Biegemodul of 3.9 GPa | ASTM D790 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 117 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 117 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 70 MPa Show Supplier Material materials with Zugfestigkeit of 70 MPa | ASTM D638 |
Thermisch
Rheological Properties
Property | Temperature | Value |
---|---|---|
Schrumpfung | 23.0 °C | 0.4 - 0.8 % Show Supplier Material materials with Schrumpfung of 0.4 - 0.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Washing machine parts | |
Fillers | 30% Glass Fiber |