Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.36 g/cm³ Show Supplier Material materials with Dichte of 1.36 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 282 MPa Show Supplier Material materials with Biegefestigkeit of 282 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 12.8 GPa Show Supplier Material materials with Biegemodul of 12.8 GPa | ASTM D790 |
Dehnung | 23.0 °C | 2.5 % Show Supplier Material materials with Dehnung of 2.5 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 64 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 64 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 186 MPa Show Supplier Material materials with Zugfestigkeit of 186 MPa | ASTM D638 |
Thermisch
Rheological Properties
Property | Temperature | Value |
---|---|---|
Schrumpfung | 23.0 °C | 0.3 % Show Supplier Material materials with Schrumpfung of 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | New energy vehicles, smart devices, low-carbon travel equipment, mine equipment, etc. | |
Fillers | 30% Carbon Fiber |