Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.33 g/cm³ Show Supplier Material materials with Dichte of 1.33 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 485 MPa Show Supplier Material materials with Biegefestigkeit of 485 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 28 GPa Show Supplier Material materials with Biegemodul of 28 GPa | ASTM D790 |
Dehnung | 23.0 °C | 1 - 2 % Show Supplier Material materials with Dehnung of 1 - 2 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 32 GPa Show Supplier Material materials with Elastizitätsmodul of 32 GPa | ASTM D790 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 292 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 292 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 330 MPa Show Supplier Material materials with Zugfestigkeit of 330 MPa | ASTM D638 |
Thermisch
Rheological Properties
Property | Temperature | Value |
---|---|---|
Schrumpfung | 23.0 °C | 0.2 - 0.3 % Show Supplier Material materials with Schrumpfung of 0.2 - 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical/electronic applications; industrial components; automotive applications | |
Fillers | 40% Carbon Fiber |