Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.1 g/cm³ Show Supplier Material materials with Dichte of 1.1 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 60 MPa Show Supplier Material materials with Biegefestigkeit of 60 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 1.5 GPa Show Supplier Material materials with Biegemodul of 1.5 GPa | ASTM D790 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 600 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 600 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 50 MPa Show Supplier Material materials with Zugfestigkeit of 50 MPa | ASTM D638 |
Thermisch
Rheological Properties
Property | Temperature | Value |
---|---|---|
Schrumpfung | 23.0 °C | 1.4 - 1.8 % Show Supplier Material materials with Schrumpfung of 1.4 - 1.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Wheelchair wheels, floor expansion tubes, electrical enclosures, auto parts, rollers, sports equipment, etc. | |
Fillers | Molybdenum Disulfide |