Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.54 g/cm³ Show Supplier Material materials with Dichte of 1.54 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 269 MPa Show Supplier Material materials with Biegefestigkeit of 269 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 11 GPa Show Supplier Material materials with Biegemodul of 11 GPa | ASTM D790 |
Dehnung | 23.0 °C | 2.5 % Show Supplier Material materials with Dehnung of 2.5 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 110 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 110 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 183 MPa Show Supplier Material materials with Zugfestigkeit of 183 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 288 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 288 °C | ASTM D648 | |
Entflammbarkeit | UL94 v0 |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Schrumpfung | 23.0 °C | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Vacuum suction pen handle, semiconductor, bushing, bearing, seal, support ring. | |
Fillers | 30% Glass Fiber |