Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.62 g/cm³ Show Supplier Material materials with Dichte of 1.62 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 8.27 GPa Show Supplier Material materials with Biegemodul of 8.27 GPa | ASTM D790 |
Dehnung | 23.0 °C | 3 % Show Supplier Material materials with Dehnung of 3 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 64 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 64 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 115 MPa Show Supplier Material materials with Zugfestigkeit of 115 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 220 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 220 °C | ASTM D648 | |
Entflammbarkeit | UL94 V0 |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Fuseless circuit breakers, electromagnetic switches, flyback transformers, household appliances handles, connectors, housings; Fans, keyboards, parts, lampshades. Vacuum cleaner components, electric fans, hair dryer shells, coffee utensils, etc., switches, motor shells, fuse boxes, door handles, bumpers, switchboard covers, mudguards, wire protection shells, rim covers, heat dissipation Window grilles, body panels, wheel covers, door and window parts, etc. | |
Fillers | 30% Glass Fiber |