Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.32 g/cm³ Show Supplier Material materials with Dichte of 1.32 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 7.54 GPa Show Supplier Material materials with Biegemodul of 7.54 GPa | ASTM D790 |
Dehnung | 23.0 °C | 4 % Show Supplier Material materials with Dehnung of 4 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 250 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 250 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 132 MPa Show Supplier Material materials with Zugfestigkeit of 132 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 210 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C | ASTM D648 | |
Entflammbarkeit | UL94 HB |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Schrumpfung | 23.0 °C | 0.3 % Show Supplier Material materials with Schrumpfung of 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Cutting machine, electric saw, electric drill, angle grinder, polisher, electric hammer, electric pick, hot air gun, lithium battery screwdriver, sanding machine, engraving machine, etc.; cooling water chamber, intake manifold, mirror frame bracket, pass style Barriers, door handles, throttle bodies, fan covers, shift lever covers, hand brakes, accelerator pedals, gears, etc.; water pumps, water valves, bearings, bushings, gears, brackets, rollers, etc.; ski equipment, strollers, bicycles , Seat bracket, pulley, shaft, shredder gear, printer parts, etc. | |
Fillers | 33% Glass Fiber |