Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.57 g/cm³ Show Supplier Material materials with Dichte of 1.57 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 14.1 GPa Show Supplier Material materials with Biegemodul of 14.1 GPa | ASTM D790 |
Dehnung | 23.0 °C | 1.5 % Show Supplier Material materials with Dehnung of 1.5 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 32 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 32 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 159 MPa Show Supplier Material materials with Zugfestigkeit of 159 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 260 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 260 °C | ASTM D648 | |
Entflammbarkeit | UL94 V0 |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Schrumpfung | 23.0 °C | 0.2 % Show Supplier Material materials with Schrumpfung of 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Aircraft landing gear, wings, hatch, fuel tank cover, J nose cone, cabin interior and other components | |
Fillers | 30% Carbon Fiber |