Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Dichte of 1.19 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 12.4 GPa Show Supplier Material materials with Biegemodul of 12.4 GPa | ASTM D790 |
Dehnung | 23.0 °C | 4 % Show Supplier Material materials with Dehnung of 4 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 53 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 53 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 110 MPa Show Supplier Material materials with Zugfestigkeit of 110 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 104 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 104 °C | ASTM D648 | |
Entflammbarkeit | UL94 HB |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Schrumpfung | 23.0 °C | 0.15 % Show Supplier Material materials with Schrumpfung of 0.15 % |
Technological properties
Property | ||
---|---|---|
Application areas | Semiconductors, LCDs, electronic components Applications: storage trays, pads, rollers, bushings, IC parts, guide wheels, rollers, parts of precision measuring devices, electromagnetic wave stickers for low frequency numbers. | |
Fillers | 30% Carbon Fiber |