Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.47 g/cm³ Show Supplier Material materials with Dichte of 1.47 g/cm³ | ISO 1183 |
Recycled Content | 40 % Show Supplier Material materials with Recycled Content of 40 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 150 MPa Show Supplier Material materials with Biegefestigkeit of 150 MPa | ISO 178, 2 mm/min |
Biegemodul | 23.0 °C | 6.5 GPa Show Supplier Material materials with Biegemodul of 6.5 GPa | ISO 178, 2 mm/min |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | ISO 179eA |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 6 kJ/m² | ISO 180 |
Zugfestigkeit | 23.0 °C | 85 MPa Show Supplier Material materials with Zugfestigkeit of 85 MPa | ISO 527, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Aschegehalt | 23.0 °C | 20 % Show Supplier Material materials with Aschegehalt of 20 % | ASTM D5630 |
Heat deflection temperature, 1.80 MPa | 215 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 215 °C | ISO 75 | |
Schmelzpunkt | 250 °C Show Supplier Material materials with Schmelzpunkt of 250 °C | ISO 3146 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Electrical Components (e.g. Brackets & Connectors), Heat resistance handles & structural applications | |
Certifications | RoHS,RECH | |
Color | Black | |
Fillers | 40% Glass Fiber and Mineral Powder | |
Processing methods |