Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.56 g/cm³ Show Supplier Material materials with Dichte of 1.56 g/cm³ | ASTM D792 |
Recycled Content | 50 % Show Supplier Material materials with Recycled Content of 50 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 210 MPa Show Supplier Material materials with Biegefestigkeit of 210 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 10 GPa Show Supplier Material materials with Biegemodul of 10 GPa | ASTM D790 |
Impact strength, Izod notched, ASTM | 23.0 °C | 75 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 75 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 140 MPa Show Supplier Material materials with Zugfestigkeit of 140 MPa | ASTM D638 |
Thermisch
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Electrical components (e.g. brackets and connectors), structural applications (e.g. grills) and furniture. | |
Certifications | RoHS,RECH,ULE Environmental Claims Validation | |
Color | Black | |
Fillers | 35% Glass Fiber | |
Processing methods |