Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.64 g/cm³ Show Supplier Material materials with Dichte of 1.64 g/cm³ | ISO 1183 |
Recycled Content | 30 % Show Supplier Material materials with Recycled Content of 30 % | ||
Wasserabsorption | 23.0 °C | 0.06 % Show Supplier Material materials with Wasserabsorption of 0.06 % | ASTM D570, 23°C/24hr |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 177 MPa Show Supplier Material materials with Biegefestigkeit of 177 MPa | ISO 178, 2 mm/min |
Biegemodul | 23.0 °C | 10.48 GPa Show Supplier Material materials with Biegemodul of 10.48 GPa | ISO 178, 2 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 7 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 7 kJ/m² | ISO 180 |
Zugfestigkeit | 23.0 °C | 120 MPa Show Supplier Material materials with Zugfestigkeit of 120 MPa | ISO 527, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Aschegehalt | 23.0 °C | 40 % Show Supplier Material materials with Aschegehalt of 40 % | ASTM D5630 | ||
Heat deflection temperature, 1.80 MPa | 222 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 222 °C | ISO 75 | |||
Schmelzpunkt | 246 °C Show Supplier Material materials with Schmelzpunkt of 246 °C | ISO 3146 | |||
Entflammbarkeit | HB for 3.2 mm sample UL94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dissipation factor, 1kHz | 23.0 °C | 8E-3 [-] Show Supplier Material materials with Dissipation factor, 1kHz of 8E-3 [-] | ASTM D150 |
Durchschlagfestigkeit | 23.0 °C | 28.4 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 28.4 kV/mm | ASTM D149, 1.6 mm, 500V/s in oil |
Volume resistivity | 23.0 °C | 1.65E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.65E+16 Ω·cm | ASTM D257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Ignition systems,Electrical components (e.g. electric motors, brackets, connectors), structural applications (grills). | |
Certifications | RoHS,RECH,ULE Environmental Claims Validation | |
Color | Black | |
Fillers | 40% Glass Fiber and Mineral Powder | |
Processing methods |