Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.33 g/cm³ Show Supplier Material materials with Dichte of 1.33 g/cm³ | ISO 1183 |
Recycled Content | 99 % Show Supplier Material materials with Recycled Content of 99 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 90 MPa Show Supplier Material materials with Biegefestigkeit of 90 MPa | ASTM D790, 1.3 mm/min |
Biegemodul | 23.0 °C | 2.8 GPa Show Supplier Material materials with Biegemodul of 2.8 GPa | ASTM D790 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 33 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 33 kJ/m² | ISO 180 |
Streckgrenze | 23.0 °C | 58 MPa Show Supplier Material materials with Streckgrenze of 58 MPa | ASTM D638, 50 mm/min |
Thermisch
Technological properties
Property | ||
---|---|---|
Certifications | RoHS,RECH,ULE Environmental Claims Validation | |
Processing methods |