Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 12 - 15 % Show Material materials with Dehnung of 12 - 15 % |
Streckgrenze | 23.0 °C | 210 - 250 MPa Show Material materials with Streckgrenze of 210 - 250 MPa |
Zugfestigkeit | 23.0 °C | 440 - 460 MPa Show Material materials with Zugfestigkeit of 440 - 460 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | General: Gas valves and fittings, fasteners, pump trim, gears, locks, heavy-duty electrical connectors, marine hardware, transmission components, safety tools and decorative metalwork | |
Corrosion properties | A very good corrosion resistance but not as high as CZ114. | |
General machinability | Readily machinable alloy |