Allgemein
Property | Value | Shape | Related Standards |
---|---|---|---|
Dichte | 4.54 g/cm³ Show Material materials with Dichte of 4.54 g/cm³ | Sheet, Plate, Billet | |
4.54 g/cm³ Show Material materials with Dichte of 4.54 g/cm³ | Billet | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 |
Abmessung
Property | Value | Shape |
---|---|---|
Breite | 400 mm Show Material materials with Breite of 400 mm | Sheet |
600 mm Show Material materials with Breite of 600 mm | Plate | |
1524 mm Show Material materials with Breite of 1524 mm | Sheet | |
1600 mm Show Material materials with Breite of 1600 mm | Plate | |
Durchmesser | 130 mm Show Material materials with Durchmesser of 130 mm | Billet |
350 mm Show Material materials with Durchmesser of 350 mm | Billet | |
Länge | 1500 mm Show Material materials with Länge of 1500 mm | Sheet, Plate |
3000 mm Show Material materials with Länge of 3000 mm | Billet | |
4500 mm Show Material materials with Länge of 4500 mm | Billet | |
5000 mm Show Material materials with Länge of 5000 mm | Sheet | |
6500 mm Show Material materials with Länge of 6500 mm | Plate |
valueMetaData
Property | Value |
---|
Mechanisch
Property | Value | Shape | Related Standards |
---|---|---|---|
Dehnung | 10.0 % Show Material materials with Dehnung of 10.0 % | Sheet, Plate, Billet | |
Elastizitätsmodul | 114 GPa Show Material materials with Elastizitätsmodul of 114 GPa | Billet | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 |
117.0 GPa Show Material materials with Elastizitätsmodul of 117.0 GPa | Sheet, Plate, Billet | ||
Härte, Brinell | 411.0 Show Material materials with Härte, Brinell of 411.0 | Sheet, Plate, Billet | |
Härte, Rockwell C | 44.0 [-] Show Material materials with Härte, Rockwell C of 44.0 [-] | Sheet, Plate, Billet | |
Härte, Vickers | 430.0 Show Material materials with Härte, Vickers of 430.0 | Sheet, Plate, Billet | |
Poissonzahl | 0.32 [-] Show Material materials with Poissonzahl of 0.32 [-] | Sheet, Plate, Billet | |
Schlagfestigkeit, Charpy gekerbt | 16.0 - 19.0 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 16.0 - 19.0 kJ/m² | Billet | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 |
Schubmodule | 45.0 GPa Show Material materials with Schubmodule of 45.0 GPa | Sheet, Plate, Billet | |
Streckgrenze | 965.0 MPa Show Material materials with Streckgrenze of 965.0 MPa | Billet | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 |
1210.0 MPa Show Material materials with Streckgrenze of 1210.0 MPa | Sheet, Plate, Billet | ||
Zugfestigkeit | 1034.0 MPa Show Material materials with Zugfestigkeit of 1034.0 MPa | Billet | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 |
1280.0 MPa Show Material materials with Zugfestigkeit of 1280.0 MPa | Sheet, Plate, Billet |
Thermisch
Property | Temperature | Value | Related Standards | Shape |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 0.000009 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.000009 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet |
20 °C | 0.0000093 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000093 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
20 °C | 0.0000095 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000095 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
100 °C | 0.000009 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.000009 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
315 °C | 0.0000093 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000093 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
538 °C | 0.0000095 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000095 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
Schmelzpunkt | 1627.0 - 1649.0 °C Show Material materials with Schmelzpunkt of 1627.0 - 1649.0 °C | Sheet, Plate, Billet | ||
1650.0 °C Show Material materials with Schmelzpunkt of 1650.0 °C | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | ||
Spezifische Wärmekapazität | 635 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 635 J/(kg·K) | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
Wärmeleitfähigkeit | 5.5 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 5.5 W/(m·K) | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
6.6 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 6.6 W/(m·K) | Sheet, Plate, Billet |
Elektrisch
Property | Value | Related Standards | Shape |
---|---|---|---|
spezifischer Widerstand | 1.57e-06 Ω·m Show Material materials with spezifischer Widerstand of 1.57e-06 Ω·m | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 5.0 - 6.0 % Show Material materials with Aluminium of 5.0 - 6.0 % | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |
Eisen | 0.35 - 1.0 % Show Material materials with Eisen of 0.35 - 1.0 % | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |
Kohlenstoff | 0.05 Show Material materials with Kohlenstoff of 0.05 | Sheet, Plate, Billet | |
0.08 Show Material materials with Kohlenstoff of 0.08 | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
Kupfer | 0.35 - 1.0 % Show Material materials with Kupfer of 0.35 - 1.0 % | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet |
Sauerstoff | 0.2 Show Material materials with Sauerstoff of 0.2 | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |
Stickstoff | 0.04 Show Material materials with Stickstoff of 0.04 | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |
Vanadium | 5.0 - 6.0 % Show Material materials with Vanadium of 5.0 - 6.0 % | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |
Wasserstoff | 0.0125 Show Material materials with Wasserstoff of 0.0125 | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet |
0.015 Show Material materials with Wasserstoff of 0.015 | Sheet, Plate, Billet | ||
Zinn | 1.5 - 2.5 % Show Material materials with Zinn of 1.5 - 2.5 % | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |