Allgemein
Property | Value | Shape | Related Standards |
---|---|---|---|
Dichte | 4.42 g/cm³ Show Material materials with Dichte of 4.42 g/cm³ | Sheet, Plate | |
4.45 g/cm³ Show Material materials with Dichte of 4.45 g/cm³ | Billet, Tube | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 |
Abmessung
Property | Value | Shape | Related Standards |
---|---|---|---|
Breite | 400 mm Show Material materials with Breite of 400 mm | Sheet | |
600 mm Show Material materials with Breite of 600 mm | Plate | ||
1524 mm Show Material materials with Breite of 1524 mm | Sheet | ||
1600 mm Show Material materials with Breite of 1600 mm | Plate | ||
Durchmesser | 5 mm Show Material materials with Durchmesser of 5 mm | Tube | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 |
25.4 mm Show Material materials with Durchmesser of 25.4 mm | Billet | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | |
125 mm Show Material materials with Durchmesser of 125 mm | Billet | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | |
130 mm Show Material materials with Durchmesser of 130 mm | Tube | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | |
Länge | 1000 mm Show Material materials with Länge of 1000 mm | Tube | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 |
1500 mm Show Material materials with Länge of 1500 mm | Sheet, Plate | ||
5000 mm Show Material materials with Länge of 5000 mm | Sheet, Tube | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | |
6500 mm Show Material materials with Länge of 6500 mm | Plate | ||
Wall thickness | 0.5 - 9.0 mm Show Material materials with Wall thickness of 0.5 - 9.0 mm | Tube | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 |
2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | Billet | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 |
valueMetaData
Property | Value |
---|
Mechanisch
Property | Value | Shape | Related Standards |
---|---|---|---|
Dehnung | 10.0 % Show Material materials with Dehnung of 10.0 % | Sheet, Plate | |
Elastizitätsmodul | 110.0 GPa Show Material materials with Elastizitätsmodul of 110.0 GPa | Billet, Tube | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 |
114.0 GPa Show Material materials with Elastizitätsmodul of 114.0 GPa | Sheet, Plate | ||
Härte, Rockwell C | 30.0 - 35.0 [-] Show Material materials with Härte, Rockwell C of 30.0 - 35.0 [-] | Sheet | |
Härte, Vickers | 310.0 Show Material materials with Härte, Vickers of 310.0 | Sheet, Plate | |
Poissonzahl | 0.31 [-] Show Material materials with Poissonzahl of 0.31 [-] | Sheet, Plate | |
Schubmodule | 41.0 GPa Show Material materials with Schubmodule of 41.0 GPa | Sheet, Plate | |
Streckgrenze | 760.0 MPa Show Material materials with Streckgrenze of 760.0 MPa | Billet, Tube | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 |
795.0 MPa Show Material materials with Streckgrenze of 795.0 MPa | Sheet, Plate | ||
Zugfestigkeit | 825.0 - 860.0 MPa Show Material materials with Zugfestigkeit of 825.0 - 860.0 MPa | Billet, Tube | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 |
860.0 MPa Show Material materials with Zugfestigkeit of 860.0 MPa | Sheet, Plate |
Thermisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 7.699999999999999e-06 - 1e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.699999999999999e-06 - 1e-05 1/K | Typical for Titanium Alpha Beta Alloy | ||
Schmelzpunkt | 1500.0 - 1750.0 °C Show Material materials with Schmelzpunkt of 1500.0 - 1750.0 °C | Typical for Titanium Alpha Beta Alloy | ||
Spezifische Wärmekapazität | 560 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 560 J/(kg·K) | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube | |
580 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 580 J/(kg·K) | Sheet, Plate | |||
Wärmeleitfähigkeit | 6.6 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 6.6 W/(m·K) | Sheet, Plate | ||
6.9 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 6.9 W/(m·K) | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 5.5 - 6.5 % Show Material materials with Aluminium of 5.5 - 6.5 % | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Sheet, Plate, Billet, Tube |
Eisen | 0.25 Show Material materials with Eisen of 0.25 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Sheet, Plate, Billet, Tube |
Kohlenstoff | 0.08 Show Material materials with Kohlenstoff of 0.08 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Sheet, Plate, Billet, Tube |
Sauerstoff | 0.13 % Show Material materials with Sauerstoff of 0.13 % | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Sheet, Plate, Billet, Tube |
Stickstoff | 0.05 Show Material materials with Stickstoff of 0.05 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Sheet, Plate, Billet, Tube |
Vanadium | 3.5 - 4.5 % Show Material materials with Vanadium of 3.5 - 4.5 % | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Sheet, Plate, Billet, Tube |
Wasserstoff | 0.012 Show Material materials with Wasserstoff of 0.012 | Sheet, Plate | |
0.015 Show Material materials with Wasserstoff of 0.015 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |