Allgemein
Property | Value | Related Standards | Shape |
---|---|---|---|
Dichte | 4.45 g/cm³ Show Material materials with Dichte of 4.45 g/cm³ | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Abmessung
Property | Value | Related Standards | Shape |
---|---|---|---|
Durchmesser | 5 mm Show Material materials with Durchmesser of 5 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Tube |
25.4 mm Show Material materials with Durchmesser of 25.4 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet | |
125 mm Show Material materials with Durchmesser of 125 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet | |
130 mm Show Material materials with Durchmesser of 130 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Tube | |
Länge | 1000 mm Show Material materials with Länge of 1000 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Tube |
5000 mm Show Material materials with Länge of 5000 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Tube | |
Wall thickness | 0.5 - 9.0 mm Show Material materials with Wall thickness of 0.5 - 9.0 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Tube |
2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet |
Mechanisch
Property | Value | Related Standards | Shape |
---|---|---|---|
Elastizitätsmodul | 110.0 GPa Show Material materials with Elastizitätsmodul of 110.0 GPa | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Streckgrenze | 760.0 MPa Show Material materials with Streckgrenze of 760.0 MPa | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Zugfestigkeit | 825.0 - 860.0 MPa Show Material materials with Zugfestigkeit of 825.0 - 860.0 MPa | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Thermisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 7.699999999999999e-06 - 1e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.699999999999999e-06 - 1e-05 1/K | Typical for Titanium Alpha Beta Alloy | ||
Schmelzpunkt | 1500.0 - 1750.0 °C Show Material materials with Schmelzpunkt of 1500.0 - 1750.0 °C | Typical for Titanium Alpha Beta Alloy | ||
Spezifische Wärmekapazität | 560 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 560 J/(kg·K) | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube | |
Wärmeleitfähigkeit | 6.9 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 6.9 W/(m·K) | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 5.5 - 6.5 % Show Material materials with Aluminium of 5.5 - 6.5 % | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Eisen | 0.25 Show Material materials with Eisen of 0.25 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Kohlenstoff | 0.08 Show Material materials with Kohlenstoff of 0.08 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Sauerstoff | 0.13 Show Material materials with Sauerstoff of 0.13 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Stickstoff | 0.05 Show Material materials with Stickstoff of 0.05 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Vanadium | 3.5 - 4.5 % Show Material materials with Vanadium of 3.5 - 4.5 % | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Wasserstoff | 0.015 Show Material materials with Wasserstoff of 0.015 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |