Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.69 g/cm³ Show Material materials with Dichte of 7.69 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 34.2 % Show Material materials with Dehnung of 34.2 % | |
Elastizitätsmodul | 23.0 °C | 195 GPa Show Material materials with Elastizitätsmodul of 195 GPa | Typical for Austenitic Stainless Steel |
Flächenreduzierung | 20.0 °C | 26 % Show Material materials with Flächenreduzierung of 26 % | |
650.0 °C | 30 % Show Material materials with Flächenreduzierung of 30 % | ||
760.0 °C | 30 % Show Material materials with Flächenreduzierung of 30 % | ||
Härte, Brinell | 760.0 °C | 120 [-] Show Material materials with Härte, Brinell of 120 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Austenitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Austenitic Stainless Steel |
Streckgrenze | 20.0 °C | 520 MPa Show Material materials with Streckgrenze of 520 MPa | |
650.0 °C | 310 MPa Show Material materials with Streckgrenze of 310 MPa | ||
760.0 °C | 240 MPa Show Material materials with Streckgrenze of 240 MPa | ||
Zugfestigkeit | 20.0 °C | 1080 MPa Show Material materials with Zugfestigkeit of 1080 MPa | |
650.0 °C | 460 MPa Show Material materials with Zugfestigkeit of 460 MPa | ||
760.0 °C | 28 MPa Show Material materials with Zugfestigkeit of 28 MPa | ||
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 760.0 °C | 1.78E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.78E-5 1/K | The mentioned value is between 20°C and the mentioned temperature |
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Wärmeleitfähigkeit | 23.0 °C | 11 - 21 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 8.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 18 - 20 % Show Material materials with Chrom of 18 - 20 % | |
Eisen | 66.5 - 70.65 % Show Material materials with Eisen of 66.5 - 70.65 % | Balance |
Kohlenstoff | 0.3 - 0.45 % Show Material materials with Kohlenstoff of 0.3 - 0.45 % | |
Mangan | 0.8 - 1.3 % Show Material materials with Mangan of 0.8 - 1.3 % | |
Nickel | 7.5 - 8.5 % Show Material materials with Nickel of 7.5 - 8.5 % | |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % | |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % | |
Silizium | 2.75 - 3.25 % Show Material materials with Silizium of 2.75 - 3.25 % |