Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
ISO 683-1 Grade C45E quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
EN 10083-3 Grade 30MnB5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
ISO 683-2 Grade 33MnCrB5-2 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
ASTM A829 Grade 4142 As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPaGeliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
ASTM A829 Grade 4140 As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPaGeliefert von:
1 Matmatch-Lieferant
Nickel Chromium Iron Alloy
DIN 17744 Grade NiCr19NbMo precipitation hardened (+P)Medium Carbon Steel
ISO 683-1 Grade C45E normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
BS 4360 Grade 43A Hot Rolled