Mechanisch
Property | Temperature | Value |
---|---|---|
Flächenreduzierung | 20.0 °C | 16 % Show Material materials with Flächenreduzierung of 16 % |
650.0 °C | 27 % Show Material materials with Flächenreduzierung of 27 % | |
760.0 °C | 23 % Show Material materials with Flächenreduzierung of 23 % | |
Streckgrenze | 20.0 °C | 700 MPa Show Material materials with Streckgrenze of 700 MPa |
650.0 °C | 330 MPa Show Material materials with Streckgrenze of 330 MPa | |
760.0 °C | 300 MPa Show Material materials with Streckgrenze of 300 MPa | |
Zugfestigkeit | 20.0 °C | 1070 MPa Show Material materials with Zugfestigkeit of 1070 MPa |
650.0 °C | 640 MPa Show Material materials with Zugfestigkeit of 640 MPa | |
760.0 °C | 510 MPa Show Material materials with Zugfestigkeit of 510 MPa | |
Chemical properties
Property | Value |
---|---|
Chrom | 20.5 % Show Material materials with Chrom of 20.5 % |
Eisen | 63.5 - 100 % Show Material materials with Eisen of 63.5 - 100 % |
Kohlenstoff | 0.5 % Show Material materials with Kohlenstoff of 0.5 % |
Mangan | 11.5 % Show Material materials with Mangan of 11.5 % |
Niobium | 1 % Show Material materials with Niobium of 1 % |
Silizium | 0.15 % Show Material materials with Silizium of 0.15 % |
Stickstoff | 0.45 % Show Material materials with Stickstoff of 0.45 % |
Vanadium | 0.4 % Show Material materials with Vanadium of 0.4 % |
Wolfram | 2 % Show Material materials with Wolfram of 2 % |