Austenitischer rostfreier Stahl
Alloy 24 / 1.4565 Solution annealed and quenchedGeliefert von:
Hempel Special MetalsAustenitischer rostfreier Stahl
SEW 400 Grade X2CrNiMnMoNbN25-18-5-4 quenched (+Q)Austenitischer rostfreier Stahl
EN 10090 Grade X50CrMnNiNbN21-9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
EN 10090 Grade X53CrMnNiN21-9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
DIN 17480 Grade X50CrMnNiNbN21-9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
DIN 17480 Grade X53CrMnNiN21-9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
ASTM A213 Grade S34565 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A240 Grade XM-17 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A240 Grade XM-18 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A240 Grade S34565 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A479 Grade S34565 AnnealedAustenitischer rostfreier Stahl
ASTM A479 Grade XM-17 AnnealedAustenitischer rostfreier Stahl
ASTM A479 Grade XM-18 AnnealedAustenitischer rostfreier Stahl
SAE J775 Grade EV-8 For Mechanical Tests: ST+PAustenitischer rostfreier Stahl
SAE J775 Grade XEV-F For Mechanical Tests: ST+PAustenitischer rostfreier Stahl
SAE J775 Grade EV-13 For Mechanical Tests: ST+PMartensitischer Edelstahl
SEW 400 Grade X30CrMoN15-1 soft annealed (+A)Austenitischer rostfreier Stahl
ASTM A276 Grade S28200 Annealed; Hot-Finished or Cold finished