Mechanisch
Property | Temperature | Value |
---|---|---|
Flächenreduzierung | 20.0 °C | 66 % Show Material materials with Flächenreduzierung of 66 % |
760.0 °C | 31 % Show Material materials with Flächenreduzierung of 31 % | |
Streckgrenze | 20.0 °C | 360 MPa Show Material materials with Streckgrenze of 360 MPa |
760.0 °C | 170 MPa Show Material materials with Streckgrenze of 170 MPa | |
Zugfestigkeit | 20.0 °C | 800 MPa Show Material materials with Zugfestigkeit of 800 MPa |
760.0 °C | 320 MPa Show Material materials with Zugfestigkeit of 320 MPa | |
Chemical properties
Property | Value |
---|---|
Chrom | 21 % Show Material materials with Chrom of 21 % |
Eisen | 64.7 - 100 % Show Material materials with Eisen of 64.7 - 100 % |
Kohlenstoff | 0.55 % Show Material materials with Kohlenstoff of 0.55 % |
Mangan | 8.25 % Show Material materials with Mangan of 8.25 % |
Nickel | 2.8 % Show Material materials with Nickel of 2.8 % |
Silizium | 0.15 % Show Material materials with Silizium of 0.15 % |
Stickstoff | 0.45 % Show Material materials with Stickstoff of 0.45 % |
Vanadium | 0.35 % Show Material materials with Vanadium of 0.35 % |
Wolfram | 1.75 % Show Material materials with Wolfram of 1.75 % |