Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for High Carbon Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for High Carbon Steel |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for High Carbon Steel |
Schubmodule | 23.0 °C | 81 GPa Show Material materials with Schubmodule of 81 GPa | Typical for High Carbon Steel |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.32E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32E-5 1/K | Typical for High Carbon Steel |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1289 - 1478 °C Show Material materials with Schmelzpunkt of 1289 - 1478 °C | Typical for High Carbon Steel | |
Spezifische Wärmekapazität | 23.0 °C | 486 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 486 J/(kg·K) | Typical for High Carbon Steel |
Wärmeleitfähigkeit | 23.0 °C | 36 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36 W/(m·K) | Typical for High Carbon Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Chrom | 0.15 % Show Material materials with Chrom of 0.15 % |
Kohlenstoff | 0.65 - 0.7 % Show Material materials with Kohlenstoff of 0.65 - 0.7 % |
Kupfer | 0.25 % Show Material materials with Kupfer of 0.25 % |
Mangan | 0.5 - 0.8 % Show Material materials with Mangan of 0.5 - 0.8 % |
Molybdän | 0.05 % Show Material materials with Molybdän of 0.05 % |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % |
Phosphor | 0.03 - 0.04 % Show Material materials with Phosphor of 0.03 - 0.04 % |
Schwefel | 0.03 - 0.035 % Show Material materials with Schwefel of 0.03 - 0.035 % |
Silizium | 0.1 - 0.3 % Show Material materials with Silizium of 0.1 - 0.3 % |