Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Zugfestigkeit | 20.0 °C | 800 - 1000 MPa Show Material materials with Zugfestigkeit of 800 - 1000 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.6 - 1 % Show Material materials with Chrom of 0.6 - 1 % |
Kohlenstoff | 0.13 - 0.19 % Show Material materials with Kohlenstoff of 0.13 - 0.19 % |
Kupfer | 0.4 % Show Material materials with Kupfer of 0.4 % |
Mangan | 0.7 - 1 % Show Material materials with Mangan of 0.7 - 1 % |
Nickel | 0.8 - 1.1 % Show Material materials with Nickel of 0.8 - 1.1 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 0.15 - 0.4 % Show Material materials with Silizium of 0.15 - 0.4 % |