Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 15.2 % Show Material materials with Dehnung of 15.2 % | Predicted Value, Transverse | |||
16.6 % Show Material materials with Dehnung of 16.6 % | Predicted Value, A200 | ||||
18.1 % Show Material materials with Dehnung of 18.1 % | Predicted Value, A80 | ||||
18.4 % Show Material materials with Dehnung of 18.4 % | Predicted Value, A5 | ||||
19.0 % Show Material materials with Dehnung of 19.0 % | Predicted Value, A80 Transverse | ||||
20.1 % Show Material materials with Dehnung of 20.1 % | Predicted Value, A50 | ||||
20.7 % Show Material materials with Dehnung of 20.7 % | Predicted Value | ||||
Elastizitätsmodul | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Chromium Molybdenum Steel | |||
Flächenreduzierung | 41.7 % Show Material materials with Flächenreduzierung of 41.7 % | Predicted Value, Transverse | |||
42.9 % Show Material materials with Flächenreduzierung of 42.9 % | Predicted Value | ||||
Poissonzahl | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Chromium Molybdenum Steel | |||
Scherfestigkeit | 514.4 MPa Show Material materials with Scherfestigkeit of 514.4 MPa | Predicted Value | |||
Schubmodule | 79.6 GPa Show Material materials with Schubmodule of 79.6 GPa | Predicted Value | |||
Zugfestigkeit | 480 MPa Show Material materials with Zugfestigkeit of 480 MPa | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.1e-05 - 1.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1e-05 - 1.4e-05 1/K | Typical for Chromium Molybdenum Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel |
Spezifische Wärmekapazität | 448 - 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Wärmeleitfähigkeit | 36 - 43 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.8 - 1.1 % Show Material materials with Chrom of 0.8 - 1.1 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Kohlenstoff | 0.36 - 0.44 % Show Material materials with Kohlenstoff of 0.36 - 0.44 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Mangan | 0.75 - 1 % Show Material materials with Mangan of 0.75 - 1 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Molybdän | 0.15 - 0.25 % Show Material materials with Molybdän of 0.15 - 0.25 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Schwefel | 0.04 % Show Material materials with Schwefel of 0.04 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Silizium | 0.15 - 0.35 % Show Material materials with Silizium of 0.15 - 0.35 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |