Medium Carbon Steel
EN 10028-3 Grade P355N normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-6 Grade S620QL1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S690QL1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S460QL quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S460QL1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S500QL1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S550QL quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S620QL quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S690QL quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-6 Grade P690QH quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-5 Grade P355ML1 thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-5 Grade P420ML2 thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-5 Grade P460ML2 thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
EN 10083-3 Grade 30MnB5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
ASTM A829 Grade 4142 As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPaGeliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
ASTM A829 Grade 4140 As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPaGeliefert von:
1 Matmatch-Lieferant
Unclassified Carbon Steel
ASTM A516 Grade 450 As-Rolled or Normalized and/or Stress RelievedGeliefert von:
1 Matmatch-Lieferant
Unclassified Carbon Steel
ASTM A516 Grade 485 As-Rolled or Normalized and/or Stress RelievedGeliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
DIN 1629 Grade St 52.0 normalized or normalized formed (+N)