Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.6 - 2.7 g/cm³ Show Material materials with Dichte of 2.6 - 2.7 g/cm³ | Typical for Cast 5xx.x Series Aluminium |
Mechanisch
Property | Value | Comment |
---|---|---|
Elastizitätsmodul | 68.0 - 70.0 GPa Show Material materials with Elastizitätsmodul of 68.0 - 70.0 GPa | Typical for Cast 5xx.x Series Aluminium |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 5xx.x Series Aluminium |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.3e-05 - 2.5e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3e-05 - 2.5e-05 1/K | Typical for Cast 5xx.x Series Aluminium |
Schmelzpunkt | 450.0 - 640.0 °C Show Material materials with Schmelzpunkt of 450.0 - 640.0 °C | Typical for Cast 5xx.x Series Aluminium |
Spezifische Wärmekapazität | 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 963.0 J/(kg·K) | Typical for Cast 5xx.x Series Aluminium |
Wärmeleitfähigkeit | 60.0 - 140.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 60.0 - 140.0 W/(m·K) | Typical for Cast 5xx.x Series Aluminium |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Blei | 0.1 % Show Material materials with Blei of 0.1 % | EN 1676 |
Eisen | 0.4 % Show Material materials with Eisen of 0.4 % | EN 1676 |
0.45 - 0.9 % Show Material materials with Eisen of 0.45 - 0.9 % | EN 1676 | |
Kupfer | 0.03 % Show Material materials with Kupfer of 0.03 % | EN 1676 |
0.08 % Show Material materials with Kupfer of 0.08 % | EN 1676 | |
Magnesium | 2.7 - 3.5 % Show Material materials with Magnesium of 2.7 - 3.5 % | EN 1676 |
8.5 - 10.5 % Show Material materials with Magnesium of 8.5 - 10.5 % | EN 1676 | |
Mangan | 0.45 % Show Material materials with Mangan of 0.45 % | EN 1676 |
0.55 % Show Material materials with Mangan of 0.55 % | EN 1676 | |
Nickel | 0.1 % Show Material materials with Nickel of 0.1 % | EN 1676 |
Silizium | 0.45 % Show Material materials with Silizium of 0.45 % | EN 1676 |
2.5 % Show Material materials with Silizium of 2.5 % | EN 1676 | |
Titan | 0.15 % Show Material materials with Titan of 0.15 % | EN 1676 |
Zink | 0.1 % Show Material materials with Zink of 0.1 % | EN 1676 |
0.25 % Show Material materials with Zink of 0.25 % | EN 1676 | |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % | EN 1676 |