About Avon Metals

manufacturer of specification Aluminium & Copper alloy ingots and a physical processor and trader of scrap Aluminium, Copper, Nickel and Cobalt revert alloys and an extensive range of exotic minor metals including Chromium, conflict-free Tantalum, Niobium, Molybdenum, Tungsten, Rhenium, Hafnium, Zirconium, Vanadium, Manganese, Silicon and Magnesium.

Company profile

Headquarters

Gloucester, United Kingdom

Type

Manufacturer and Processor

Certifications

ISO 9001

, ISO 14001

, ISO 50001

Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

AFNOR A-S2GT

Ingot

AFNOR A-S2GT, EN AB-41000, EN AB-AlSi2MgTi

EN AB-21000

Ingot

EN AB-21000, EN AB-AlCu4MgTi

EN AB-21100

Ingot

EN AB-21100, EN AB-AlCu4Ti

EN AB-42000

Ingot

EN AB-42000, EN AB-AlSi7Mg

EN AB-42100

Ingot

EN AB-42100, EN AB-AlSi7Mg0.3

EN AB-42200

Ingot

EN AB-42200, EN AB-AlSi7Mg0.6

EN AB-43000

Ingot

EN AB-43000, EN AB-AlSi10Mg(A)

EN AB-43100

Ingot

EN AB-43100, EN AB-AlSi10Mg(B)

EN AB-43200

Ingot

EN AB-43200, EN AB-AlSi10Mg(Cu)

EN AB-43300

Ingot

EN AB-43300, EN AB-AlSi9Mg