Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.96 - 7.98 g/cm³ Show Material materials with Dichte of 7.96 - 7.98 g/cm³ |
50.0 °C | 7.96 g/cm³ Show Material materials with Dichte of 7.96 g/cm³ | |
100.0 °C | 7.94 g/cm³ Show Material materials with Dichte of 7.94 g/cm³ | |
150.0 °C | 7.92 g/cm³ Show Material materials with Dichte of 7.92 g/cm³ | |
200.0 °C | 7.9 g/cm³ Show Material materials with Dichte of 7.9 g/cm³ | |
250.0 °C | 7.88 g/cm³ Show Material materials with Dichte of 7.88 g/cm³ | |
300.0 °C | 7.86 g/cm³ Show Material materials with Dichte of 7.86 g/cm³ | |
350.0 °C | 7.83 g/cm³ Show Material materials with Dichte of 7.83 g/cm³ | |
400.0 °C | 7.81 g/cm³ Show Material materials with Dichte of 7.81 g/cm³ | |
450.0 °C | 7.79 g/cm³ Show Material materials with Dichte of 7.79 g/cm³ | |
500.0 °C | 7.76 g/cm³ Show Material materials with Dichte of 7.76 g/cm³ | |
550.0 °C | 7.74 g/cm³ Show Material materials with Dichte of 7.74 g/cm³ | |
600.0 °C | 7.71 g/cm³ Show Material materials with Dichte of 7.71 g/cm³ | |
650.0 °C | 7.68 g/cm³ Show Material materials with Dichte of 7.68 g/cm³ | |
700.0 °C | 7.66 g/cm³ Show Material materials with Dichte of 7.66 g/cm³ | |
750.0 °C | 7.63 g/cm³ Show Material materials with Dichte of 7.63 g/cm³ | |
800.0 °C | 7.61 g/cm³ Show Material materials with Dichte of 7.61 g/cm³ | |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 22 - 35 % Show Material materials with Dehnung of 22 - 35 % |
Elastizitätsmodul | -100.0 °C | 206 GPa Show Material materials with Elastizitätsmodul of 206 GPa |
20.0 °C | 196 - 199.44 GPa Show Material materials with Elastizitätsmodul of 196 - 199.44 GPa | |
50.0 °C | 197.57 GPa Show Material materials with Elastizitätsmodul of 197.57 GPa | |
100.0 °C | 190 - 193.65 GPa Show Material materials with Elastizitätsmodul of 190 - 193.65 GPa | |
150.0 °C | 189.43 GPa Show Material materials with Elastizitätsmodul of 189.43 GPa | |
200.0 °C | 182 - 184.82 GPa Show Material materials with Elastizitätsmodul of 182 - 184.82 GPa | |
250.0 °C | 180.11 GPa Show Material materials with Elastizitätsmodul of 180.11 GPa | |
300.0 °C | 174 - 175.5 GPa Show Material materials with Elastizitätsmodul of 174 - 175.5 GPa | |
350.0 °C | 170.89 GPa Show Material materials with Elastizitätsmodul of 170.89 GPa | |
400.0 °C | 166 - 167 GPa Show Material materials with Elastizitätsmodul of 166 - 167 GPa | |
450.0 °C | 162.26 GPa Show Material materials with Elastizitätsmodul of 162.26 GPa | |
500.0 °C | 158 - 159 GPa Show Material materials with Elastizitätsmodul of 158 - 159 GPa | |
550.0 °C | 154.02 GPa Show Material materials with Elastizitätsmodul of 154.02 GPa | |
600.0 °C | 149.99 - 150 GPa Show Material materials with Elastizitätsmodul of 149.99 - 150 GPa | |
650.0 °C | 146.07 GPa Show Material materials with Elastizitätsmodul of 146.07 GPa | |
700.0 °C | 142 - 142.05 GPa Show Material materials with Elastizitätsmodul of 142 - 142.05 GPa | |
750.0 °C | 138.32 GPa Show Material materials with Elastizitätsmodul of 138.32 GPa | |
800.0 °C | 134 - 134.69 GPa Show Material materials with Elastizitätsmodul of 134 - 134.69 GPa | |
900.0 °C | 127 GPa Show Material materials with Elastizitätsmodul of 127 GPa | |
1000.0 °C | 120 GPa Show Material materials with Elastizitätsmodul of 120 GPa | |
Poissonzahl | 20.0 °C | 0.28 [-] Show Material materials with Poissonzahl of 0.28 [-] |
50.0 °C | 0.28 [-] Show Material materials with Poissonzahl of 0.28 [-] | |
100.0 °C | 0.28 [-] Show Material materials with Poissonzahl of 0.28 [-] | |
150.0 °C | 0.28 [-] Show Material materials with Poissonzahl of 0.28 [-] | |
200.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | |
250.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | |
300.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | |
350.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | |
400.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | |
450.0 °C | 0.31 [-] Show Material materials with Poissonzahl of 0.31 [-] | |
500.0 °C | 0.31 [-] Show Material materials with Poissonzahl of 0.31 [-] | |
550.0 °C | 0.32 [-] Show Material materials with Poissonzahl of 0.32 [-] | |
600.0 °C | 0.32 [-] Show Material materials with Poissonzahl of 0.32 [-] | |
650.0 °C | 0.32 [-] Show Material materials with Poissonzahl of 0.32 [-] | |
700.0 °C | 0.32 [-] Show Material materials with Poissonzahl of 0.32 [-] | |
750.0 °C | 0.32 [-] Show Material materials with Poissonzahl of 0.32 [-] | |
800.0 °C | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | |
Schubmodule | 20.0 °C | 77.01 - 78.09 GPa Show Material materials with Schubmodule of 77.01 - 78.09 GPa |
50.0 °C | 77.3 GPa Show Material materials with Schubmodule of 77.3 GPa | |
100.0 °C | 75.73 GPa Show Material materials with Schubmodule of 75.73 GPa | |
150.0 °C | 73.87 GPa Show Material materials with Schubmodule of 73.87 GPa | |
200.0 °C | 71.91 GPa Show Material materials with Schubmodule of 71.91 GPa | |
250.0 °C | 69.95 GPa Show Material materials with Schubmodule of 69.95 GPa | |
300.0 °C | 67.89 GPa Show Material materials with Schubmodule of 67.89 GPa | |
350.0 °C | 65.83 GPa Show Material materials with Schubmodule of 65.83 GPa | |
400.0 °C | 63.96 GPa Show Material materials with Schubmodule of 63.96 GPa | |
450.0 °C | 62.1 GPa Show Material materials with Schubmodule of 62.1 GPa | |
500.0 °C | 60.33 GPa Show Material materials with Schubmodule of 60.33 GPa | |
550.0 °C | 58.57 GPa Show Material materials with Schubmodule of 58.57 GPa | |
600.0 °C | 56.9 GPa Show Material materials with Schubmodule of 56.9 GPa | |
650.0 °C | 55.33 GPa Show Material materials with Schubmodule of 55.33 GPa | |
700.0 °C | 53.86 GPa Show Material materials with Schubmodule of 53.86 GPa | |
750.0 °C | 52.29 GPa Show Material materials with Schubmodule of 52.29 GPa | |
800.0 °C | 50.82 GPa Show Material materials with Schubmodule of 50.82 GPa | |
Streckgrenze Rp 0,2 | 20.0 °C | 205 MPa Show Material materials with Streckgrenze Rp 0,2 of 205 MPa |
100.0 °C | 175 MPa Show Material materials with Streckgrenze Rp 0,2 of 175 MPa | |
200.0 °C | 157 MPa Show Material materials with Streckgrenze Rp 0,2 of 157 MPa | |
300.0 °C | 137 MPa Show Material materials with Streckgrenze Rp 0,2 of 137 MPa | |
400.0 °C | 128 MPa Show Material materials with Streckgrenze Rp 0,2 of 128 MPa | |
500.0 °C | 118 MPa Show Material materials with Streckgrenze Rp 0,2 of 118 MPa | |
550.0 °C | 118 MPa Show Material materials with Streckgrenze Rp 0,2 of 118 MPa | |
600.0 °C | 113 MPa Show Material materials with Streckgrenze Rp 0,2 of 113 MPa | |
Streckgrenze Rp 1,0 | 20.0 °C | 245 MPa Show Material materials with Streckgrenze Rp 1,0 of 245 MPa |
100.0 °C | 205 MPa Show Material materials with Streckgrenze Rp 1,0 of 205 MPa | |
200.0 °C | 186 MPa Show Material materials with Streckgrenze Rp 1,0 of 186 MPa | |
300.0 °C | 167 MPa Show Material materials with Streckgrenze Rp 1,0 of 167 MPa | |
400.0 °C | 157 MPa Show Material materials with Streckgrenze Rp 1,0 of 157 MPa | |
500.0 °C | 147 MPa Show Material materials with Streckgrenze Rp 1,0 of 147 MPa | |
550.0 °C | 147 MPa Show Material materials with Streckgrenze Rp 1,0 of 147 MPa | |
600.0 °C | 142 MPa Show Material materials with Streckgrenze Rp 1,0 of 142 MPa | |
Zugfestigkeit | 20.0 °C | 510 - 690 MPa Show Material materials with Zugfestigkeit of 510 - 690 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | -100.0 °C | 1.49E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.49E-5 1/K | |
20.0 °C | 1.61E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.61E-5 1/K | ||
100.0 °C | 1.63E-5 - 1.67E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.63E-5 - 1.67E-5 1/K | ||
200.0 °C | 1.69E-5 - 1.72E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.69E-5 - 1.72E-5 1/K | ||
300.0 °C | 1.73E-5 - 1.77E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.73E-5 - 1.77E-5 1/K | ||
400.0 °C | 1.78E-5 - 1.81E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.78E-5 - 1.81E-5 1/K | ||
500.0 °C | 1.82E-5 - 1.84E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.82E-5 - 1.84E-5 1/K | ||
600.0 °C | 1.85E-5 - 1.88E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.85E-5 - 1.88E-5 1/K | ||
700.0 °C | 1.87E-5 - 1.91E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.87E-5 - 1.91E-5 1/K | ||
800.0 °C | 1.94E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.94E-5 1/K | ||
900.0 °C | 1.97E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.97E-5 1/K | ||
1000.0 °C | 2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2E-5 1/K | ||
Max. Betriebstemperatur, lang | 0 - 800 °C Show Material materials with Max. Betriebstemperatur, lang of 0 - 800 °C | ||
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | -100.0 °C | 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 440 J/(kg·K) | |
20.0 °C | 450 - 472 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 450 - 472 J/(kg·K) | ||
100.0 °C | 487 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 487 J/(kg·K) | ||
200.0 °C | 503 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 503 J/(kg·K) | ||
300.0 °C | 512 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 512 J/(kg·K) | ||
400.0 °C | 520 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 520 J/(kg·K) | ||
500.0 °C | 530 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 530 J/(kg·K) | ||
600.0 °C | 541 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 541 J/(kg·K) | ||
700.0 °C | 551 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 551 J/(kg·K) | ||
800.0 °C | 559 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 559 J/(kg·K) | ||
900.0 °C | 565 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 565 J/(kg·K) | ||
1000.0 °C | 571 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 571 J/(kg·K) | ||
Temperaturleitfähigkeit | 20.0 °C | 3.5 mm²/s Show Material materials with Temperaturleitfähigkeit of 3.5 mm²/s | |
100.0 °C | 3.8 mm²/s Show Material materials with Temperaturleitfähigkeit of 3.8 mm²/s | ||
200.0 °C | 4 mm²/s Show Material materials with Temperaturleitfähigkeit of 4 mm²/s | ||
300.0 °C | 4.3 mm²/s Show Material materials with Temperaturleitfähigkeit of 4.3 mm²/s | ||
400.0 °C | 4.5 mm²/s Show Material materials with Temperaturleitfähigkeit of 4.5 mm²/s | ||
500.0 °C | 4.7 mm²/s Show Material materials with Temperaturleitfähigkeit of 4.7 mm²/s | ||
600.0 °C | 4.8 mm²/s Show Material materials with Temperaturleitfähigkeit of 4.8 mm²/s | ||
700.0 °C | 5.1 mm²/s Show Material materials with Temperaturleitfähigkeit of 5.1 mm²/s | ||
800.0 °C | 5.4 mm²/s Show Material materials with Temperaturleitfähigkeit of 5.4 mm²/s | ||
Wärmeleitfähigkeit | 20.0 °C | 13.3 - 16 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 13.3 - 16 W/(m·K) | |
100.0 °C | 14.9 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14.9 W/(m·K) | ||
200.0 °C | 16.5 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 16.5 W/(m·K) | ||
300.0 °C | 18.1 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 18.1 W/(m·K) | ||
400.0 °C | 19.5 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 19.5 W/(m·K) | ||
500.0 °C | 21 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 21 W/(m·K) | ||
600.0 °C | 22.4 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 22.4 W/(m·K) | ||
700.0 °C | 23.8 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 23.8 W/(m·K) | ||
800.0 °C | 25.2 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 25.2 W/(m·K) | ||
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 7.38E-7 - 7.91E-7 Ω·m Show Material materials with spezifischer Widerstand of 7.38E-7 - 7.91E-7 Ω·m |
50.0 °C | 7.61E-7 Ω·m Show Material materials with spezifischer Widerstand of 7.61E-7 Ω·m | |
100.0 °C | 7.99E-7 - 8.45E-7 Ω·m Show Material materials with spezifischer Widerstand of 7.99E-7 - 8.45E-7 Ω·m | |
150.0 °C | 8.38E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.38E-7 Ω·m | |
200.0 °C | 8.72E-7 - 9.19E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.72E-7 - 9.19E-7 Ω·m | |
250.0 °C | 9.04E-7 Ω·m Show Material materials with spezifischer Widerstand of 9.04E-7 Ω·m | |
300.0 °C | 9.34E-7 - 9.77E-7 Ω·m Show Material materials with spezifischer Widerstand of 9.34E-7 - 9.77E-7 Ω·m | |
350.0 °C | 9.63E-7 Ω·m Show Material materials with spezifischer Widerstand of 9.63E-7 Ω·m | |
400.0 °C | 9.91E-7 - 1.03E-6 Ω·m Show Material materials with spezifischer Widerstand of 9.91E-7 - 1.03E-6 Ω·m | |
450.0 °C | 1.02E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.02E-6 Ω·m | |
500.0 °C | 1.04E-6 - 1.08E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.04E-6 - 1.08E-6 Ω·m | |
550.0 °C | 1.06E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.06E-6 Ω·m | |
600.0 °C | 1.08E-6 - 1.12E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.08E-6 - 1.12E-6 Ω·m | |
650.0 °C | 1.1E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.1E-6 Ω·m | |
700.0 °C | 1.12E-6 - 1.15E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.12E-6 - 1.15E-6 Ω·m | |
750.0 °C | 1.14E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.14E-6 Ω·m | |
800.0 °C | 1.15E-6 - 1.18E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.15E-6 - 1.18E-6 Ω·m | |
Chemical properties
Property | Value |
---|---|
Chrom | 15 - 17 % Show Material materials with Chrom of 15 - 17 % |
Kohlenstoff | 0.04 - 0.1 % Show Material materials with Kohlenstoff of 0.04 - 0.1 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Nickel | 12 - 14 % Show Material materials with Nickel of 12 - 14 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.3 - 0.6 % Show Material materials with Silizium of 0.3 - 0.6 % |