Spezifische Wärmekapazität: 565 J/(kg·K)

Quick Comparison

Kohlenstoffarmer Stahl

EN 10028-2 Grade P295GH normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Kohlenstoffarmer Stahl

EN 10028-2 Grade P355GH normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Chromium Molybdenum Steel

EN 10028-2 Grade 10CrMo9-10 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMo4-5 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Molybdenum Steel

EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Molybdenum Steel

EN 10028-2 Grade 20MnMoNi4-5 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 10CrMo9-10 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMo4-5 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

ISO 683-1 Grade C45E quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Nickel molybdenum Steel

EN 10028-2 Grade 15NiCuMoNb5-6-4 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Austenitischer rostfreier Stahl

Sandvik 253 MA

Geliefert von:

Alleima (formerly Sandvik Materials Technology)

Austenitischer rostfreier Stahl

Esshete 1250

Geliefert von:

Alleima (formerly Sandvik Materials Technology)

Nickel Chromium Iron Alloy

VDM® Alloy 825

Geliefert von:

VDM Metals

Pure/Low Nickel Alloy

VDM® Alloy 200

Geliefert von:

VDM Metals

Pure/Low Nickel Alloy

VDM® Alloy 201

Geliefert von:

VDM Metals

Austenitischer rostfreier Stahl

Sandvik 2RE69

Geliefert von:

Alleima (formerly Sandvik Materials Technology)
Seite 1 von 47