Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy, V-notch | -12 °C | 27 J Show Material materials with Charpy impact energy, V-notch of 27 J | average |
4 °C | 27 J Show Material materials with Charpy impact energy, V-notch of 27 J | average | |
21 °C | 27 J Show Material materials with Charpy impact energy, V-notch of 27 J | average | |
Dehnung | 18 - 21 % Show Material materials with Dehnung of 18 - 21 % | ||
Zugfestigkeit | 485 MPa Show Material materials with Zugfestigkeit of 485 MPa | min. |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.01 - 0.04 % Show Material materials with Aluminium of 0.01 - 0.04 % | |
Chrom | 0.45 - 0.7 % Show Material materials with Chrom of 0.45 - 0.7 % | |
Kohlenstoff | 0.11 % Show Material materials with Kohlenstoff of 0.11 % | max. |
Kupfer | 0.25 - 0.4 % Show Material materials with Kupfer of 0.25 - 0.4 % | |
Mangan | 1.1 - 1.5 % Show Material materials with Mangan of 1.1 - 1.5 % | |
Molybdän | 0.02 - 0.08 % Show Material materials with Molybdän of 0.02 - 0.08 % | |
Nickel | 0.25 - 0.4 % Show Material materials with Nickel of 0.25 - 0.4 % | |
Phosphor | 0.2 % Show Material materials with Phosphor of 0.2 % | max. |
Schwefel | 0.006 % Show Material materials with Schwefel of 0.006 % | max. |
Silizium | 0.3 - 0.5 % Show Material materials with Silizium of 0.3 - 0.5 % | |
Stickstoff | 0.015 % Show Material materials with Stickstoff of 0.015 % | max. |
Vanadium | 0.04 - 0.08 % Show Material materials with Vanadium of 0.04 - 0.08 % |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |