Kohlenstoffarmer Stahl
EN 10025-3 Grade S355N normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10025-3 Grade S355NL normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10025-3 Grade S275N normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10025-3 Grade S275NL normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Nickel Molybdenum Steel
EN 10028-2 Grade 20MnMoNi4-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S550QL1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S620QL1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S690QL1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-4 Grade S275M thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-4 Grade S275ML thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-4 Grade S355M thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-4 Grade S355ML thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-6 Grade S460Q quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S460QL quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S460QL1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S500Q quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S500QL quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S500QL1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S550Q quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S550QL quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant