Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | typical for low carbon steel |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 20 - 22 % Show Material materials with Dehnung of 20 - 22 % | min. values depending on the thickness |
Elastizitätsmodul | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | typical for low carbon steel |
Poissonzahl | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | typical for low carbon steel |
Schubmodule | 82 GPa Show Material materials with Schubmodule of 82 GPa | typical for low carbon steel |
Streckgrenze | 275 - 380 MPa Show Material materials with Streckgrenze of 275 - 380 MPa | ReH, min. values depending on the thickness, If not apparent, the yield strength Rp0.2 is measured |
Zugfestigkeit | 485 - 690 MPa Show Material materials with Zugfestigkeit of 485 - 690 MPa | range depending on the thickness |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.32e-05 - 1.38e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32e-05 - 1.38e-05 1/K | typical for low carbon steel |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | typical for carbon steel |
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | typical for low carbon steel |
Spezifische Wärmekapazität | 465 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 465 J/(kg·K) | typical for low carbon steel |
Wärmeleitfähigkeit | 25 - 93 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 25 - 93 W/(m·K) | typical for low carbon steel |
Elektrisch
Property | Value | Comment |
---|---|---|
spezifischer Widerstand | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with spezifischer Widerstand of 1.43e-07 - 1.74e-07 Ω·m | typical for carbon steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 0.25 - 0.29 % Show Material materials with Chrom of 0.25 - 0.29 % | depending on analysis |
Kohlenstoff | 0.24 % Show Material materials with Kohlenstoff of 0.24 % | |
Kupfer | 0.35 - 0.38 % Show Material materials with Kupfer of 0.35 - 0.38 % | depending on analysis |
Mangan | 0.64 - 1.72 % Show Material materials with Mangan of 0.64 - 1.72 % | depending on analysis and thickness |
Molybdän | 0.08 - 0.09 % Show Material materials with Molybdän of 0.08 - 0.09 % | depending on analysis |
Nickel | 0.25 - 0.28 % Show Material materials with Nickel of 0.25 - 0.28 % | depending on analysis |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | max. |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % | max. |
Silizium | 0.13 - 0.55 % Show Material materials with Silizium of 0.13 - 0.55 % | depending on analysis |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |