Nickel: 0.25 - 0.28 %

Quick Comparison

Chromium Molybdenum Steel

EN 10028-2 Grade 12CrMoV12-10 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMoV9-10 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Kohlenstoffarmer Stahl

ASTM A612 As-Rolled or Normalized and/or Stress Relieved

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00

Chromium Molybdenum Steel

ASTM A542 Type E Class 4 Quenched and Tempered

Geliefert von:

1 Matmatch-Lieferant

Unclassified Stainless Steel

ASTM A537 Class 1 Normalized

Geliefert von:

2 Matmatch-Lieferanten

Chromium Molybdenum Steel

ASTM A542 Type D Class 1 Quenched and Tempered

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

ASTM A542 Type B Class 1 Quenched and Tempered

Geliefert von:

1 Matmatch-Lieferant

Martensitischer Edelstahl

ASTM A841 Grade A Class 1 Thermo-Mechanical Control Process (TMCP)

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper High Copper Alloy

ASTM B251 Grade C17000 TD04

Wrought Copper High Copper Alloy

ASTM B196 Grade C17000 TF00

Wrought Copper High Copper Alloy

ASTM B196 Grade C17000 TB00

Wrought Copper High Copper Alloy

ASTM B196 Grade C17000 TH04

Wrought Copper High Copper Alloy

ASTM B643 Grade C17200 TH04