Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 17.1 % Show Material materials with Dehnung of 17.1 % | Predicted Value, A200 | ||||
17.5 % Show Material materials with Dehnung of 17.5 % | Predicted Value, A80 | |||||
19.7 % Show Material materials with Dehnung of 19.7 % | Predicted Value, A80 Transverse | |||||
20.1 % Show Material materials with Dehnung of 20.1 % | Predicted Value, A5 | |||||
20.9 % Show Material materials with Dehnung of 20.9 % | Predicted Value, Transverse | |||||
23.2 % Show Material materials with Dehnung of 23.2 % | Predicted Value, A50 | |||||
20 °C | 19 % Show Material materials with Dehnung of 19 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
Elastizitätsmodul | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel | ||||
Flächenreduzierung | 42.7 % Show Material materials with Flächenreduzierung of 42.7 % | Predicted Value | ||||
44.7 % Show Material materials with Flächenreduzierung of 44.7 % | Predicted Value, Transverse | |||||
Härte, Brinell | 245 [-] Show Material materials with Härte, Brinell of 245 [-] | Predicted Value, Transverse | ||||
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel | ||||
Scherfestigkeit | 529 MPa Show Material materials with Scherfestigkeit of 529 MPa | Predicted Value | ||||
Schubmodule | 80.3 GPa Show Material materials with Schubmodule of 80.3 GPa | Predicted Value | ||||
Streckgrenze | 251.3 MPa Show Material materials with Streckgrenze of 251.3 MPa | Predicted Value, RP1 | ||||
318.7 MPa Show Material materials with Streckgrenze of 318.7 MPa | Predicted Value, RP1 Transverse | |||||
418.3 MPa Show Material materials with Streckgrenze of 418.3 MPa | Predicted Value, RP02 | |||||
422.5 MPa Show Material materials with Streckgrenze of 422.5 MPa | Predicted Value, Transverse | |||||
472.4 MPa Show Material materials with Streckgrenze of 472.4 MPa | Predicted Value, RP02 Transverse | |||||
485.4 MPa Show Material materials with Streckgrenze of 485.4 MPa | Predicted Value, RP002 | |||||
501.4 MPa Show Material materials with Streckgrenze of 501.4 MPa | Predicted Value, RP05 | |||||
20 °C | 365 MPa Show Material materials with Streckgrenze of 365 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 370 MPa Show Material materials with Streckgrenze of 370 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 380 MPa Show Material materials with Streckgrenze of 380 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 390 MPa Show Material materials with Streckgrenze of 390 MPa | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
20 °C | 400 MPa Show Material materials with Streckgrenze of 400 MPa | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
20 °C | 420 MPa Show Material materials with Streckgrenze of 420 MPa | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
Zugfestigkeit | 20 °C | 460 - 680 MPa Show Material materials with Zugfestigkeit of 460 - 680 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | |
20 °C | 460 - 660 MPa Show Material materials with Zugfestigkeit of 460 - 660 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 460 - 650 MPa Show Material materials with Zugfestigkeit of 460 - 650 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 460 - 630 MPa Show Material materials with Zugfestigkeit of 460 - 630 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 460 - 620 MPa Show Material materials with Zugfestigkeit of 460 - 620 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 470 - 680 MPa Show Material materials with Zugfestigkeit of 470 - 680 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 470 - 660 MPa Show Material materials with Zugfestigkeit of 470 - 660 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 470 - 650 MPa Show Material materials with Zugfestigkeit of 470 - 650 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 470 - 630 MPa Show Material materials with Zugfestigkeit of 470 - 630 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 470 - 620 MPa Show Material materials with Zugfestigkeit of 470 - 620 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 480 - 680 MPa Show Material materials with Zugfestigkeit of 480 - 680 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 480 - 660 MPa Show Material materials with Zugfestigkeit of 480 - 660 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 480 - 650 MPa Show Material materials with Zugfestigkeit of 480 - 650 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 480 - 630 MPa Show Material materials with Zugfestigkeit of 480 - 630 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 480 - 620 MPa Show Material materials with Zugfestigkeit of 480 - 620 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 500 - 660 MPa Show Material materials with Zugfestigkeit of 500 - 660 MPa | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
20 °C | 500 - 680 MPa Show Material materials with Zugfestigkeit of 500 - 680 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 500 - 650 MPa Show Material materials with Zugfestigkeit of 500 - 650 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 500 - 630 MPa Show Material materials with Zugfestigkeit of 500 - 630 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 500 - 620 MPa Show Material materials with Zugfestigkeit of 500 - 620 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 520 - 680 MPa Show Material materials with Zugfestigkeit of 520 - 680 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 520 - 660 MPa Show Material materials with Zugfestigkeit of 520 - 660 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 520 - 650 MPa Show Material materials with Zugfestigkeit of 520 - 650 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 520 - 630 MPa Show Material materials with Zugfestigkeit of 520 - 630 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 520 - 620 MPa Show Material materials with Zugfestigkeit of 520 - 620 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 11.87 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 11.87 1/K | Predicted Value |
Spezifische Wärmekapazität | 455.7 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 455.7 J/(kg·K) | Predicted Value |
Wärmeleitfähigkeit | 38.02 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 38.02 W/(m·K) | Predicted Value |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Chrom | 0.3 % Show Material materials with Chrom of 0.3 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
Kohlenstoff | 0.16 % Show Material materials with Kohlenstoff of 0.16 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Kupfer | 0.55 % Show Material materials with Kupfer of 0.55 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
Mangan | 1.7 % Show Material materials with Mangan of 1.7 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Molybdän | 0.2 % Show Material materials with Molybdän of 0.2 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar |
0.8 % Show Material materials with Nickel of 0.8 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
0.035 % Show Material materials with Phosphor of 0.035 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar | |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
0.03 % Show Material materials with Schwefel of 0.03 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar | |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Stickstoff | 0.02 % Show Material materials with Stickstoff of 0.02 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar |
0.025 % Show Material materials with Stickstoff of 0.025 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | |
Titan | 0.05 % Show Material materials with Titan of 0.05 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Vanadium | 0.12 % Show Material materials with Vanadium of 0.12 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |