Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 12.2 % Show Material materials with Dehnung of 12.2 % | Predicted Value, A200 | ||||
15.1 % Show Material materials with Dehnung of 15.1 % | Predicted Value, A80 | |||||
17.6 % Show Material materials with Dehnung of 17.6 % | Predicted Value, Transverse | |||||
19.2 % Show Material materials with Dehnung of 19.2 % | Predicted Value, A80 Transverse | |||||
20.2 % Show Material materials with Dehnung of 20.2 % | Predicted Value, A5 | |||||
22.6 % Show Material materials with Dehnung of 22.6 % | Predicted Value, A50 | |||||
20 °C | 17 % Show Material materials with Dehnung of 17 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
Elastizitätsmodul | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel | ||||
Flächenreduzierung | 41.9 % Show Material materials with Flächenreduzierung of 41.9 % | Predicted Value | ||||
44.6 % Show Material materials with Flächenreduzierung of 44.6 % | Predicted Value, Transverse | |||||
Härte, Brinell | 246 [-] Show Material materials with Härte, Brinell of 246 [-] | Predicted Value, Transverse | ||||
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel | ||||
Scherfestigkeit | 528.9 MPa Show Material materials with Scherfestigkeit of 528.9 MPa | Predicted Value | ||||
Schubmodule | 80.3 GPa Show Material materials with Schubmodule of 80.3 GPa | Predicted Value | ||||
Streckgrenze | 257.3 MPa Show Material materials with Streckgrenze of 257.3 MPa | Predicted Value, RP1 | ||||
319.9 MPa Show Material materials with Streckgrenze of 319.9 MPa | Predicted Value, RP1 Transverse | |||||
430.3 MPa Show Material materials with Streckgrenze of 430.3 MPa | Predicted Value, RP02 | |||||
438.2 MPa Show Material materials with Streckgrenze of 438.2 MPa | Predicted Value, Transverse | |||||
472.8 MPa Show Material materials with Streckgrenze of 472.8 MPa | Predicted Value, RP02 Transverse | |||||
515.9 MPa Show Material materials with Streckgrenze of 515.9 MPa | Predicted Value, RP05 | |||||
516.7 MPa Show Material materials with Streckgrenze of 516.7 MPa | Predicted Value, RP002 | |||||
20 °C | 385 MPa Show Material materials with Streckgrenze of 385 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 400 MPa Show Material materials with Streckgrenze of 400 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 410 MPa Show Material materials with Streckgrenze of 410 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 430 MPa Show Material materials with Streckgrenze of 430 MPa | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
20 °C | 440 MPa Show Material materials with Streckgrenze of 440 MPa | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
20 °C | 460 MPa Show Material materials with Streckgrenze of 460 MPa | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
Zugfestigkeit | 20 °C | 490 - 720 MPa Show Material materials with Zugfestigkeit of 490 - 720 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | |
20 °C | 490 - 710 MPa Show Material materials with Zugfestigkeit of 490 - 710 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 490 - 690 MPa Show Material materials with Zugfestigkeit of 490 - 690 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 490 - 680 MPa Show Material materials with Zugfestigkeit of 490 - 680 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 490 - 660 MPa Show Material materials with Zugfestigkeit of 490 - 660 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 500 - 720 MPa Show Material materials with Zugfestigkeit of 500 - 720 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 500 - 710 MPa Show Material materials with Zugfestigkeit of 500 - 710 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 500 - 690 MPa Show Material materials with Zugfestigkeit of 500 - 690 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 500 - 680 MPa Show Material materials with Zugfestigkeit of 500 - 680 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 500 - 660 MPa Show Material materials with Zugfestigkeit of 500 - 660 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 510 - 720 MPa Show Material materials with Zugfestigkeit of 510 - 720 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 510 - 710 MPa Show Material materials with Zugfestigkeit of 510 - 710 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 510 - 690 MPa Show Material materials with Zugfestigkeit of 510 - 690 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 510 - 680 MPa Show Material materials with Zugfestigkeit of 510 - 680 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 510 - 660 MPa Show Material materials with Zugfestigkeit of 510 - 660 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 530 - 720 MPa Show Material materials with Zugfestigkeit of 530 - 720 MPa | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
20 °C | 530 - 710 MPa Show Material materials with Zugfestigkeit of 530 - 710 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 530 - 690 MPa Show Material materials with Zugfestigkeit of 530 - 690 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 530 - 680 MPa Show Material materials with Zugfestigkeit of 530 - 680 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 530 - 660 MPa Show Material materials with Zugfestigkeit of 530 - 660 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 540 - 720 MPa Show Material materials with Zugfestigkeit of 540 - 720 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 540 - 710 MPa Show Material materials with Zugfestigkeit of 540 - 710 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 540 - 690 MPa Show Material materials with Zugfestigkeit of 540 - 690 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 540 - 680 MPa Show Material materials with Zugfestigkeit of 540 - 680 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 540 - 660 MPa Show Material materials with Zugfestigkeit of 540 - 660 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 11.84 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 11.84 1/K | Predicted Value |
Spezifische Wärmekapazität | 455.2 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 455.2 J/(kg·K) | Predicted Value |
Wärmeleitfähigkeit | 37.88 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 37.88 W/(m·K) | Predicted Value |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Chrom | 0.3 % Show Material materials with Chrom of 0.3 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
Kohlenstoff | 0.16 % Show Material materials with Kohlenstoff of 0.16 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Kupfer | 0.55 % Show Material materials with Kupfer of 0.55 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
Mangan | 1.7 % Show Material materials with Mangan of 1.7 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Molybdän | 0.2 % Show Material materials with Molybdän of 0.2 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Nickel | 0.45 % Show Material materials with Nickel of 0.45 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar |
0.8 % Show Material materials with Nickel of 0.8 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
0.03 % Show Material materials with Phosphor of 0.03 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar | |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
0.025 % Show Material materials with Schwefel of 0.025 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar | |
Silizium | 0.6 % Show Material materials with Silizium of 0.6 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Stickstoff | 0.025 % Show Material materials with Stickstoff of 0.025 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Titan | 0.05 % Show Material materials with Titan of 0.05 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Vanadium | 0.12 % Show Material materials with Vanadium of 0.12 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |