Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 40 % Show Material materials with Dehnung of 40 % | |
Dehnung A80 | 20.0 °C | 37 % Show Material materials with Dehnung A80 of 37 % | |
Elastizitätsmodul | 23.0 °C | 195 GPa Show Material materials with Elastizitätsmodul of 195 GPa | Typical for Austenitic Stainless Steel |
Härte, Brinell | 20.0 °C | 210 [-] Show Material materials with Härte, Brinell of 210 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Austenitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Austenitic Stainless Steel |
Streckgrenze Rp 0,2 | 20.0 °C | 310 MPa Show Material materials with Streckgrenze Rp 0,2 of 310 MPa | |
Streckgrenze Rp 1,0 | 20.0 °C | 350 MPa Show Material materials with Streckgrenze Rp 1,0 of 350 MPa | |
Zugfestigkeit | 20.0 °C | 650 - 850 MPa Show Material materials with Zugfestigkeit of 650 - 850 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 200.0 °C | 1.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 1/K | |
400.0 °C | 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | ||
600.0 °C | 1.85E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.85E-5 1/K | ||
800.0 °C | 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.9E-5 1/K | ||
1000.0 °C | 1.95E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.95E-5 1/K | ||
Max. Betriebstemperatur, lang | 0 - 1150 °C Show Material materials with Max. Betriebstemperatur, lang of 0 - 1150 °C | ||
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 20.0 °C | 500 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 500 J/(kg·K) | |
600.0 °C | 660 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 660 J/(kg·K) | ||
Wärmeleitfähigkeit | 20.0 °C | 15 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 15 W/(m·K) | |
500.0 °C | 21 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 21 W/(m·K) | ||
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 8.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.5E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Cerium | 0.03 - 0.08 % Show Material materials with Cerium of 0.03 - 0.08 % |
Chrom | 20 - 22 % Show Material materials with Chrom of 20 - 22 % |
Kohlenstoff | 0.05 - 0.12 % Show Material materials with Kohlenstoff of 0.05 - 0.12 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 10 - 12 % Show Material materials with Nickel of 10 - 12 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 1.4 - 2.5 % Show Material materials with Silizium of 1.4 - 2.5 % |
Stickstoff | 0.12 - 0.2 % Show Material materials with Stickstoff of 0.12 - 0.2 % |