Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.85 g/cm³ Show Material materials with Dichte of 7.85 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 20 % Show Material materials with Dehnung of 20 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Steel |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Steel |
Schubmodule | 23.0 °C | 76 GPa Show Material materials with Schubmodule of 76 GPa | Typical for Nickel Steel |
Streckgrenze Rp 0,2 | 20.0 °C | 360 MPa Show Material materials with Streckgrenze Rp 0,2 of 360 MPa | |
100.0 °C | 255 MPa Show Material materials with Streckgrenze Rp 0,2 of 255 MPa | ||
150.0 °C | 235 MPa Show Material materials with Streckgrenze Rp 0,2 of 235 MPa | ||
200.0 °C | 215 MPa Show Material materials with Streckgrenze Rp 0,2 of 215 MPa | ||
250.0 °C | 190 MPa Show Material materials with Streckgrenze Rp 0,2 of 190 MPa | ||
300.0 °C | 175 MPa Show Material materials with Streckgrenze Rp 0,2 of 175 MPa | ||
Zugfestigkeit | 20.0 °C | 500 - 650 MPa Show Material materials with Zugfestigkeit of 500 - 650 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | -195.0 °C | 8.5E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.5E-6 1/K | |
-170.0 °C | 9E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9E-6 1/K | ||
-120.0 °C | 9.8E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9.8E-6 1/K | ||
-50.0 °C | 1.04E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.04E-5 1/K | ||
-25.0 °C | 1.06E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.06E-5 1/K | ||
Max. Betriebstemperatur, lang | -90 - 0 °C Show Material materials with Max. Betriebstemperatur, lang of -90 - 0 °C | ||
Schmelzpunkt | 1316 - 1595 °C Show Material materials with Schmelzpunkt of 1316 - 1595 °C | Typical for Nickel Steel | |
Spezifische Wärmekapazität | 20.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | |
Wärmeleitfähigkeit | -20.0 °C | 35 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 35 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 0.3 % Show Material materials with Chrom of 0.3 % |
Kohlenstoff | 0.06 - 0.12 % Show Material materials with Kohlenstoff of 0.06 - 0.12 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 0.5 - 0.8 % Show Material materials with Mangan of 0.5 - 0.8 % |
Molybdän | 0.2 % Show Material materials with Molybdän of 0.2 % |
Nickel | 3 - 4 % Show Material materials with Nickel of 3 - 4 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.6 % Show Material materials with Silizium of 0.6 % |
Vanadium | 0.05 % Show Material materials with Vanadium of 0.05 % |