Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 16 % Show Material materials with Dehnung of 16 % | |
Dehnung, transversal | 20.0 °C | 14 % Show Material materials with Dehnung, transversal of 14 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 20.0 °C | 500 - 620 MPa Show Material materials with Streckgrenze of 500 - 620 MPa | |
Streckgrenze Rp 0,2 | 100.0 °C | 430 - 490 MPa Show Material materials with Streckgrenze Rp 0,2 of 430 - 490 MPa | |
150.0 °C | 420 - 480 MPa Show Material materials with Streckgrenze Rp 0,2 of 420 - 480 MPa | ||
200.0 °C | 410 - 470 MPa Show Material materials with Streckgrenze Rp 0,2 of 410 - 470 MPa | ||
250.0 °C | 400 - 460 MPa Show Material materials with Streckgrenze Rp 0,2 of 400 - 460 MPa | ||
300.0 °C | 390 - 450 MPa Show Material materials with Streckgrenze Rp 0,2 of 390 - 450 MPa | ||
Streckgrenze, transversal | 20.0 °C | 500 - 620 MPa Show Material materials with Streckgrenze, transversal of 500 - 620 MPa | |
Zugfestigkeit | 20.0 °C | 630 - 930 MPa Show Material materials with Zugfestigkeit of 630 - 930 MPa | |
100.0 °C | 540 - 640 MPa Show Material materials with Zugfestigkeit of 540 - 640 MPa | ||
150.0 °C | 520 - 620 MPa Show Material materials with Zugfestigkeit of 520 - 620 MPa | ||
200.0 °C | 500 - 600 MPa Show Material materials with Zugfestigkeit of 500 - 600 MPa | ||
250.0 °C | 500 - 600 MPa Show Material materials with Zugfestigkeit of 500 - 600 MPa | ||
300.0 °C | 500 - 600 MPa Show Material materials with Zugfestigkeit of 500 - 600 MPa | ||
Zugfestigkeit, transversal | 20.0 °C | 630 - 930 MPa Show Material materials with Zugfestigkeit, transversal of 630 - 930 MPa |
Thermisch
Property | Value |
---|---|
Max. Betriebstemperatur, lang | -20 - 300 °C Show Material materials with Max. Betriebstemperatur, lang of -20 - 300 °C |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Chrom | 0.3 % Show Material materials with Chrom of 0.3 % |
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 1 - 1.7 % Show Material materials with Mangan of 1 - 1.7 % |
Molybdän | 0.1 % Show Material materials with Molybdän of 0.1 % |
Nickel | 0.8 % Show Material materials with Nickel of 0.8 % |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 0.6 % Show Material materials with Silizium of 0.6 % |
Stickstoff | 0.02 % Show Material materials with Stickstoff of 0.02 % |
Titan | 0.04 % Show Material materials with Titan of 0.04 % |
Vanadium | 0.2 % Show Material materials with Vanadium of 0.2 % |