Unclassified Low Alloy Steel
EN 10025-6 Grade S550QL1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S620QL1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S620Q quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S620QL quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S690Q quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S690QL quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S960Q quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-6 Grade P690QL1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-6 Grade P690QL2 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-6 Grade P690Q quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-6 Grade P690QH quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
ISO 683-2 Grade 33MnCrB5-2 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10149-2 Grade S650MC thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10149-2 Grade S700MC thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
ASTM A542 Type A Class 2 Quenched and TemperedGeliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
ASTM A542 Type D Class 1 Quenched and TemperedGeliefert von:
1 Matmatch-Lieferant
Ferritischer Edelstahl
SEW 400 Grade X20CrMo13 quenched and tempered (+QT)Kohlenstoffarmer Stahl
EN 10297-1 Grade 36Mn4 quenched and tempered (+QT)Martensitischer Edelstahl
DIN 17440 Grade X17CrNi16-2 quenched and tempered (+QT)Medium Carbon Steel
EN 10297-1 Grade C55 quenched and tempered (+QT)