Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.85 g/cm³ Show Material materials with Dichte of 7.85 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 22 % Show Material materials with Dehnung of 22 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 20.0 °C | 315 - 355 MPa Show Material materials with Streckgrenze of 315 - 355 MPa | |
Streckgrenze Rp 0,2 | 50.0 °C | 280 - 340 MPa Show Material materials with Streckgrenze Rp 0,2 of 280 - 340 MPa | |
100.0 °C | 250 - 310 MPa Show Material materials with Streckgrenze Rp 0,2 of 250 - 310 MPa | ||
150.0 °C | 225 - 285 MPa Show Material materials with Streckgrenze Rp 0,2 of 225 - 285 MPa | ||
200.0 °C | 200 - 260 MPa Show Material materials with Streckgrenze Rp 0,2 of 200 - 260 MPa | ||
250.0 °C | 175 - 235 MPa Show Material materials with Streckgrenze Rp 0,2 of 175 - 235 MPa | ||
300.0 °C | 155 - 215 MPa Show Material materials with Streckgrenze Rp 0,2 of 155 - 215 MPa | ||
Zugfestigkeit | 20.0 °C | 450 - 630 MPa Show Material materials with Zugfestigkeit of 450 - 630 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.018 % Show Material materials with Aluminium of 0.018 % |
Bor | 5E-3 % Show Material materials with Bor of 5E-3 % |
Chrom | 0.3 % Show Material materials with Chrom of 0.3 % |
Kohlenstoff | 0.16 % Show Material materials with Kohlenstoff of 0.16 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Molybdän | 0.25 % Show Material materials with Molybdän of 0.25 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.01 - 0.015 % Show Material materials with Schwefel of 0.01 - 0.015 % |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % |
Stickstoff | 0.02 % Show Material materials with Stickstoff of 0.02 % |
Titan | 0.03 % Show Material materials with Titan of 0.03 % |
Vanadium | 0.06 % Show Material materials with Vanadium of 0.06 % |
Zirkonium | 0.05 % Show Material materials with Zirkonium of 0.05 % |