Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 12 % Show Material materials with Dehnung A50 of 12 % | |
Elastizitätsmodul | 23.0 °C | 190 GPa Show Material materials with Elastizitätsmodul of 190 GPa | |
Härte, Brinell | 23.0 °C | 190 [-] Show Material materials with Härte, Brinell of 190 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for High Carbon Steel |
Schubmodule | 23.0 °C | 81 GPa Show Material materials with Schubmodule of 81 GPa | Typical for High Carbon Steel |
Zugfestigkeit | 23.0 °C | 1620 - 3480 MPa Show Material materials with Zugfestigkeit of 1620 - 3480 MPa | For Different Diameters |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.2E-5 1/K | |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1410 °C Show Material materials with Schmelzpunkt of 1410 °C | ||
Spezifische Wärmekapazität | 23.0 °C | 470 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 470 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 36 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36 W/(m·K) | Typical for High Carbon Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.6 - 0.95 % Show Material materials with Kohlenstoff of 0.6 - 0.95 % |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % |
Mangan | 0.3 - 0.9 % Show Material materials with Mangan of 0.3 - 0.9 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.12 - 0.32 % Show Material materials with Silizium of 0.12 - 0.32 % |
Technological properties
Property | ||
---|---|---|
Application areas | Piano (Music) Wire | |
Corrosion properties | Not Corrosion Resistance |