Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.8 g/cm³ Show Material materials with Dichte of 8.8 g/cm³ | Typical for Nickel Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 8 - 35 % Show Material materials with Dehnung A5 of 8 - 35 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Steel |
Härte, Brinell | 23.0 °C | 262 - 321 [-] Show Material materials with Härte, Brinell of 262 - 321 [-] | |
Härte, Rockwell C | 23.0 °C | 26 - 35 [-] Show Material materials with Härte, Rockwell C of 26 - 35 [-] | |
Härte, Vickers | 23.0 °C | 270 - 335 [-] Show Material materials with Härte, Vickers of 270 - 335 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Steel |
Schubmodule | 23.0 °C | 76 GPa Show Material materials with Schubmodule of 76 GPa | Typical for Nickel Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 615 MPa Show Material materials with Streckgrenze Rp 0,2 of 615 MPa | |
Zugfestigkeit | 23.0 °C | 930 - 960 MPa Show Material materials with Zugfestigkeit of 930 - 960 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 1316 - 1595 °C Show Material materials with Schmelzpunkt of 1316 - 1595 °C | Typical for Nickel Steel | |
Spezifische Wärmekapazität | 23.0 °C | 456 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 456 J/(kg·K) | Typical for Nickel Steel |
Wärmeleitfähigkeit | 23.0 °C | 10 - 50 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 10 - 50 W/(m·K) | Typical for Nickel Steel |
Technological properties
Property | ||
---|---|---|
Processing history | ageing treatment after solution treatment |